Technical Data Sheet
Specification | Hardness at 23oC | Density at 23oC (g/cm3) | Tensile Strength (Mpa) | Elongation at breatk (%) |
---|---|---|---|---|
Test Method | ASTM D2240 | ASTM D792 | IEC 811-1-1 | IEC 811-1-1 |
Unit | Shore A | g/cm3 | Mpa | % |
NHMP247 | 90 | 1.35 | 18.8 | 330.8 |
Technical Data Sheet
Specification | Hardness at 23oC | Density at 23oC (g/cm3) | Tensile Strength (Mpa) | Elongation at breatk (%) |
---|---|---|---|---|
Test Method | ASTM D2240 | ASTM D792 | IEC 811-1-1 | IEC 811-1-1 |
Unit | Shore A | g/cm3 | Mpa | % |
NHMP247 | 90 | 1.35 | 18.8 | 330.8 |